TECHNET Archives

November 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Tue, 12 Nov 2013 14:26:09 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Depends: heavy metal or tin pan?
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Tuesday, November 12, 2013 7:17 AM
To: [log in to unmask]
Subject: [TN] NTC cleaning gold finish

OK, the topic sounds like it could be on topic......

I have a new guitar.  The electronics are cool, could be ENiG, but...

The real question is the Tuners.  They are very thin gold plate over Nickel (sound familiar?).  I have heard people suggest cleaning them with Naptha (or lighter fluid).  I figured who would know better than the gurus here if that's a good idea.

Naptha on Gold over Nickel - good or bad idea?

Pete

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2