Here is a thought, this is from the mechanical side. What diameter is
bored in the board? Fashion a go-no go gauge that is the bore of the
hole minus the minimum thickness plating allowed. If it fits it is a
no go, you can also make one with the bore minus the maximum thickness
allowed.
Also known as a pin-gauge, we used these all the time to verify
calibration of crimping tools that require a minimum crush factor.
pat
On Thu, Nov 21, 2013 at 10:40 AM, Stadem, Richard D. wrote:
> Can't you microsection a solder coupon and measure using SEM?
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
> Sent: Thursday, November 21, 2013 10:23 AM
> To: [log in to unmask]
> Subject: [TN] rental of PTH plating thickness gauge
>
> TechNetters, I want to rent a gauge for measuring copper plating
> thickness in circuit board plated through holes. Oxford used to rent
> its CMI 511, but no longer does so. Any suggestions about where to go
> for that or a comparable gage? I haven't had much success via the
> internet.
>
> Thanks for any help.
>
> Louis Hart
> Compunetics
> Monroeville, PA
> USA
> [log in to unmask]<mailto:[log in to unmask]>
> 412-858-1232
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|