It depends how much gold on the surface. With nowadays, not much (with the price over 1000.00).
Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Frederick Miller
Sent: Tuesday, November 12, 2013 3:34 PM
To: [log in to unmask]
Subject: Re: [TN] NTC cleaning gold finish
You can not harm the gold with any solvent that you can buy in a super market unless it is an abrasive cleaner. No steel wool or wire brush.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Tuesday, November 12, 2013 2:57 PM
To: [log in to unmask]
Subject: Re: [TN] NTC cleaning gold finish
Gee, to diminish the discord here, understand these are not A flat finish, but high gloss. A minor problem, but I would like them to B sharp looking, as they augment the look of the instrument, and sustain it's value.
(Don't fret, Dewey, you're still the head nut here)
And I am sure the IPA idea to improve the sound would work, especially if applied liberally to my audience.
But really, will Naptha harm the Gold?
Pete
This e-mail message and any attachments may contain confidential information from Astrolab Inc. If you are not the intended recipient, you are hereby notified that disclosure, printing, copying, distribution, or the taking of any action in reliance on the contents of this electronic information is strictly prohibited. If you have received this e-mail message in error, please immediately notify the sender by reply message and then delete the electronic message and any attachments. Thank you for your cooperation.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|