Lots of variables here.
Please provide more detail.
Chuck
Charles W. Brummer | 3M Manufacturing Engineer
3M Electronic Solutions Division
3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com
This message (including any attachments) may contain material, non-public
information or proprietary information and is for the intended recipients
only. If you are not the intended recipient, you should notify the sender
and delete this message. Any disclosure, copying, or use of this
information is strictly prohibited and may subject you to legal liability.
From: Ramakrishnan Saravanan <[log in to unmask]>
To: <[log in to unmask]>
Date: 10/31/2013 05:35 AM
Subject: [TN] MLB LAMINATION TEMPERATIRE
Sent by: TechNet <[log in to unmask]>
The Laminate suppliers specification for lamination is 183 deg C at 90
minutes. We are laminating at 190 deg C for 90 minutes. This is to ensure
complete cure. We are pressing single stack at a time. Is there any
reliability concerns ?.
R.Saravanan
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________