Sorry Joyce, but I have to disagree: "Gummy" doesn't tell the full story of how a material reacts to ultrasonic bonding. You could stick down a device with a wet paste of cornstarch and it would bond fine: The material just needs adequate stiffness at the bonding frequency, and most bonding candidates should be adequate, especially if you keep the bonding line thin.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Tuesday, October 08, 2013 10:53 AM
To: [log in to unmask]
Subject: Re: [TN] Thermally conductive adhesive/epoxy
If you want to bond parts and followed by ultrasonic bonding, you don't want gummy stuff. How much money you have? BN or diamond filled might be on the order. To bond flex - polyimide or copper pads? Totally different requirements.
Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Tuesday, October 08, 2013 10:22 AM
To: [log in to unmask]
Subject: [TN] Thermally conductive adhesive/epoxy
Good Morning All,
I am looking for some kind of thermally conductive system to bond a piece of Aluminum onto a flex circuit. The Aluminum will act as a heat sink/spreader. We will then SMT some parts on the top of the flex and then ultrasonic bond a flip chip. If a supplier wants to contact me offline- (416) 750-8433.
Thanks. Steve Kelly
If the recipient to whom this e-mail is sent has an NDA with PFC Flexible Circuits Limited this e-mail is considered confidential and is subject to any NDA agreements between the respective parties.
See PFC on "How It's Made`` coming soon on the Discovery Channel!
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|