TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="us-ascii"
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 1 Oct 2013 15:41:58 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Krug <[log in to unmask]>
Subject:
From:
Richard Krug <[log in to unmask]>
Message-ID:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (16 lines)
Due to business acquisitions we now have an assembly that has been assembled using SMT adhesive followed by wave soldering.  
I know larger multilayer ceramic capacitors are subject to cracking due to thermal shock.  Is there a similar concern with large chip resistors.  

Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL  34602-8299
p (352) 540-4012  (Internal Ext. 2012)
[log in to unmask]

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2