Subject: Re: [TN] Bonding to PTFE
Thanks technetters for the guidance on the pretreating option. In another life corona and flame treatment were also options (but not so for PCB
applications)
Bob W
On Tue, Oct 22, 2013 at 9:09 AM, Bob Wettermann <[log in to unmask]> wrote:
> Can a chemist/board SME tell me if an epoxy/resin system will bond to
> a PTFE matrix laminate for pad/trace repair?
>
> Thanks!
>
> Bob Wettermann
>
--
1. Bob Wettermann
847-767-5745
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________