TECHNET Archives

September 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 3 Sep 2013 06:09:05 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (80 lines)
This does not involve ENIG as it a large flat aluminum sheet metal with a layer of nickel..
Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, August 29, 2013 6:19 PM
To: [log in to unmask]
Subject: Re: [TN] Solder joint failure

Hi TechNet - the gold plating of an ENIG surface finish is primarily protecting the underlying nickel from oxidation so that an active flux is not required to produce a solder joint. During soldering the gold diffuses into the solder allowing a tin/nickel intermetallic phase to form creating the basis for a metallurgical joint. If the nickel gets oxidized, then a highly active flux is typically needed to allow the same reaction to occur.

Dave Hillman
Rockwell Collins
[log in to unmask]


From:   Robert Kondner <[log in to unmask]>
To:     <[log in to unmask]>
Date:   08/29/2013 03:03 PM
Subject:        Re: [TN] Solder joint failure
Sent by:        TechNet <[log in to unmask]>


I agree. The flux makes a big difference.

 I regularly solder to nickel tabs that are spot welded to battery cells.
I
played with various flux materials, the thick RMA flux from flux pens has worked best. I have also solder coated by dipping in a solder pot, that RMA works well.

 This always concerned me about ENIG, once the gold is dissolved off the surface what happens next?

 Bob K.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Thursday, August 29, 2013 3:01 PM
To: [log in to unmask]
Subject: Re: [TN] Solder joint failure

In my experience nickel is NOT easy to solder to at all.


-----Original Message-----
From: Victor Hernandez [mailto:[log in to unmask]]
Sent: Thursday, August 29, 2013 2:53 PM
To: [log in to unmask]
Subject: [TN] Solder joint failure

Fellow TechNetters:

   Should I be concern with an electroless matted nickel plating over an aluminum sheet metal surface and solder onto a copper heat tube?   I
recall something about directly soldering onto a nickel surface.  Beside nickel oxidation.    Any suggestions would be greatly appreciated.

Victor,

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2