Hi Mumtaz,
Thanks, I'll take a look at it!
Brs,
Gerry
> Date: Thu, 19 Sep 2013 16:38:33 +0000
> From: [log in to unmask]
> Subject: Re: [TN] FW: [TN] Test procedure(s) sought for outgassing of volatiles from plastics
> To: [log in to unmask]
>
> Hi Gerry, There is a residual gas analysis procedure from JEDEC--JEP144A for micorelectronic packages.
>
>
> Thank-you
> Mumtaz
> 858-795-0112
> Peregrine Semiconductor
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerry Gagnon
> Sent: Thursday, September 19, 2013 9:04 AM
> To: [log in to unmask]
> Subject: [TN] FW: [TN] Test procedure(s) sought for outgassing of volatiles from plastics
>
> Hi All,
>
> While not as interesting as bugs in soldermask ( I actually have a pic of a mouse that somehow got laminated into a 6 layer board somewhere in my files).........
> I was hoping someone could respond to the message below and give me a specification reference that they've used and trusted so I don't wind up re-developing the "outgassing of plastics" wheel....
>
> Brs,
>
> Gerry
>
> > Date: Wed, 18 Sep 2013 09:43:36 -0400
> > From: [log in to unmask]
> > Subject: [TN] Test procedure(s) sought for outgassing of volatiles
> > from plastics
> > To: [log in to unmask]
> >
> > Hi Technet,
> >
> > I've run into some sensors that may be susceptible to deposition of outgassed volatiles from plastic housings, esd bags, tapes, and adhesives.
> >
> > I'm not looking "space" type protection, however, some of these materials cooking in your trunk on a hot day will outgas things that are not good for sensors.
> >
> > Is there a procedure out there to test for outgassing in earthly environments?
> >
> > Thanks and best regards,
> >
> > Gerry
> >
> >
> > ______________________________________________________________________
> > This email has been scanned by the Symantec Email Security.cloud service.
> > For more information please contact helpdesk at x2960 or
> > [log in to unmask]
> > ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
>
>
> CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|