Hi Folks,
How many times can be allowed to re-balling BGA?
Lyon Yuan
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, September 05, 2013 12:29 AM
To: [log in to unmask]
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Unless it was reballed and placed and soldered. The second heat cycle of removal may have caused the pad to come off.
From: Bob Wettermann [mailto:[log in to unmask]]
Sent: Wednesday, September 04, 2013 11:24 AM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Gents:
Lyon wrote "Bob,
After removed BGA, we found pad of BGA was missing." From what the patient is telling us it happened UPON REMOVAL (not during reballing process) Bob W
On Wed, Sep 4, 2013 at 11:18 AM, Stadem, Richard D. <[log in to unmask]<mailto:[log in to unmask]>> wrote:
I don't think so, as then the other pads would also display varying degrees of erosion. This appears to be a pad that was lifted during the reballing process, as part of the pad prep after rework (removal of the old solder).
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Gumpert, Ben
Sent: Wednesday, September 04, 2013 9:20 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop Or potentially too much time at liquidus dissolved the pad away, or left minimal pad that was easily lifted.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Steve Gregory
Sent: Wednesday, September 04, 2013 10:16 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop Well, well, well....there's your answer. I think someone did not have a delicate touch when they cleaned the pads...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Lyon Yuan
Sent: Wednesday, September 4, 2013 8:14 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Hi Steve
Yes, it was re-balled
Lyon Yuan
From: stephen gregory [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Wednesday, September 04, 2013 10:11 PM
To: Lyon Yuan; TechNet E-Mail Forum
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Hi Lyon!
Have your picture posted, it's here:
http://stevezeva.homestead.com/Pad_missing.JPG
Do you know if this BGA was re-balled?
Steve
From: Lyon Yuan <[log in to unmask]<mailto:[log in to unmask]>>
To: 'stephen gregory' <[log in to unmask]<mailto:[log in to unmask]>>; 'Steve Gregory' <[log in to unmask]<mailto:[log in to unmask]>>
Sent: Wednesday, September 4, 2013 8:00 AM
Subject: RE: [TN] EXTERNAL: [TN] BGA pad drop
Steve,
Help to upload picture to web. Thanks
Lyon Yuan
-----Original Message-----
From: Wenger, George M. [Contractor] [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Wednesday, September 04, 2013 9:54 PM
To: Lyon Yuan
Cc: stephen gregory; Steve Gregory
Subject: RE: [TN] EXTERNAL: [TN] BGA pad drop
Lyon,
Attached is a link to his site. The last emails I had for Steve are on the copy to line of this email <http://stevezeva.homestead.com/> http://stevezeva.homestead.com/
Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771<tel:%28908%29%20638-8771> Home (732) 309-8964<tel:%28732%29%20309-8964> Mobile
E-mail: <mailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]>
<mailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]>
-----Original Message-----
From: Lyon Yuan [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Wednesday, September 04, 2013 9:45 AM
To: Wenger, George M. [Contractor]
Subject: RE: [TN] EXTERNAL: [TN] BGA pad drop
George
Thanks, steve's email?
Lyon Yuan
-----Original Message-----
From: Wenger, George M. [Contractor] [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Wednesday, September 04, 2013 9:35 PM
To: TechNet E-Mail Forum; Lyon Yuan
Subject: RE: [TN] EXTERNAL: [TN] BGA pad drop
Hi Lyon,
You might want to send the picture to Steve to post on his site so we all can see it.
Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771<tel:%28908%29%20638-8771> Home (732) 309-8964<tel:%28732%29%20309-8964> Mobile
E-mail: <mailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]>
<mailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Lyon Yuan
Sent: Wednesday, September 04, 2013 9:32 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Hi Ben,
I send a clear picture for your reference
Lyon Yuan
-----Original Message-----
From: [log in to unmask]<mailto:[log in to unmask]> [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Gumpert, Ben
Sent: Wednesday, September 04, 2013 8:04 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Lyon,
I haven’t seen that.
Typically the pads on the BGA are solder mask defined, which makes them much more secure than the usual non-solder mask defined pads on the PWB.
Ben
From: [log in to unmask]<mailto:[log in to unmask]> [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Wednesday, September 04, 2013 7:04 AM
To: Gumpert, Ben
Cc: TechNet
Subject: Re:Re: [TN] EXTERNAL: [TN] BGA pad drop
hi ben,
it is pad missing from bga
在2013/09/04, "Gumpert, Ben" < <mailto:[log in to unmask]<mailto:[log in to unmask]>%3cmailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>>> 写道:
Lyon, By 'pad drop' do you mean lifted pads? (Pads stayed with the BGA?) Usually this means that there wasn't enough heat - that the solder was not melted in all locations. Ben -----Original Message----- From: TechNet <mailto:[mailto:[log in to unmask]<mailto:[log in to unmask]>]> [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Lyon Yuan Sent: Wednesday, September 04, 2013 6:40 AM To: <mailto:[log in to unmask]<mailto:[log in to unmask]>%3cmailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>> Subject: EXTERNAL: [TN] BGA pad drop guys,we found a few BGA pad drop after removed from pcba boards.what is reason to cause the issue ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]<mailto:[log in to unmask]>%3cmailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>> ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]<mailto:[log in to unmask]>%3cmailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]<mailto:[log in to unmask]>> [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
--
1. Bob Wettermann
847-767-5745
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|