TECHNET Archives

September 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Doug Pauls <[log in to unmask]>
Date:
Fri, 6 Sep 2013 10:11:24 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "lduso - Diamond-MT.com" <[log in to unmask]>
Message-ID:
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (154 lines)
You are correct, the 350 is the smallest and is a benchtop. I guess it
really depends on what is being dispensed. Good for conformal coating but
that was over kill for what I was looking for. I was more or less looking
for a simple robotic dispenser like Fisnar makes to dispense masking
material like liquid latex.

Jon is a great guy and definately knows his stuff. He was really helpful
with coming up with a good process for us to coat a rather strange item
from a customer.

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com


On Fri, Sep 6, 2013 at 9:01 AM, <[log in to unmask]> wrote:

> I have always found their support to be excellent and very responsive.  I
> like the fact that most of their machines are built from stock parts that
> you can get from Grainger or McMaster Carr.  Only their controllers and
> their valves are custom to PVA.  The thing that I like about the Pathmaster
> software, other than being easy to use, is that it is excellent for
> "tweaking" the program.  Editing is very easy.  Jon Merrill, their master
> programmer, REALLY knows his stuff.
>
> I am surprised to hear about the benchtop equipment.  I have one of their
> PVA350 benchtops, which I still see on their web site.  Now, the 350 is
> only a 3 axis machine, but does pretty well for adhesive dispense.  Did
> they discontinue ALL benchtops or just the 200 series?
>
> Doug Pauls
>
>
>
> From:        "lduso - Diamond-MT.com" <[log in to unmask]>
> To:        TechNet E-Mail Forum <[log in to unmask]>, Doug Pauls <
> [log in to unmask]>
> Date:        09/06/2013 07:55 AM
> Subject:        Re: [TN] Benchtop dispensers
> ------------------------------
>
>
>
> Doug
>
> I agree with the PVA comment. I was just up to their plant last month.
> Great place and good people. Unfortunately, they stopped making the
> benchtop products. It used to be their 200 series. (I know because I asked
> for one when I was there.) Their software does look like a good user
> friendly style though.
>
> Lloyd Duso
> Diamond-MT
> Plant Manager
> (814) 535-3505
> *www.Diamond-mt.com* <http://www.diamond-mt.com/>
>
>
> On Fri, Sep 6, 2013 at 8:19 AM, Douglas Pauls <*
> [log in to unmask]* <[log in to unmask]>> wrote:
> Both Nordson EFD and PVA (Precision Valve and Automation) make good
> benchtop dispense units.  Those are the two I would start with.
>
> I have more experience with the PVAs and have found PVA to be a good
> company to work with.  I really like their Pathmaster software for
> programming and editing.
>
> Doug Pauls
>
>
>
> From:   "Stadem, Richard D." <*[log in to unmask]*<[log in to unmask]>
> >
> To:     "*[log in to unmask]* <[log in to unmask]>" <*
> [log in to unmask]* <[log in to unmask]>>,
> "TechNet E-Mail Forum" <*[log in to unmask]* <[log in to unmask]>>
> Date:   09/06/2013 06:02 AM
> Subject:        RE: [TN] Benchtop dispensers
>
>
>
> Zymet TC201 thermally conductive epoxy and Loctite 3621.
>
> From: *[log in to unmask]* <[log in to unmask]> [mailto:
> *[log in to unmask]* <[log in to unmask]>]
> Sent: Thursday, September 05, 2013 3:27 PM
> To: TechNet E-Mail Forum; Stadem, Richard D.
> Subject: Re: [TN] Benchtop dispensers
>
> What do you want to dispense?
>
> Doug Pauls
>
>
>
> From:        "Stadem, Richard D." <*[log in to unmask]*<[log in to unmask]>
> >
> To:        <*[log in to unmask]* <[log in to unmask]>>
> Date:        09/05/2013 03:20 PM
> Subject:        [TN] Benchtop dispensers
> Sent by:        TechNet <*[log in to unmask]* <[log in to unmask]>>
>
>
>
>
> I am seeking feedback from Those Who Know (you folks).
> I need to purchase a benchtop dispensing robot. I am looking at something
> like a Fisnar model F2304N-1 which is a 4-axis model, X, Y, Z, and R.
> I am looking at Fisnar, EFD, Fishman, and other similar manufacturers.
> I would like feedback from the Forum as to which vendors you might
> recommend, bad experiences, what to look for, etc.
> You are always free to contact me on the Forum or offline. I will even
> take you out and buy you a few beers if you're not too far away!
> Thanks for any feedback
> dean
>
> This message and/or attachments may include information subject to GDC4S
> S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed
> only by authorized recipients. Use, storage and transmission are governed
> by General Dynamics and its policies. Contractual restrictions apply to
> third parties. Recipients should refer to the policies or contract to
> determine proper handling. Unauthorized review, use, disclosure or
> distribution is prohibited. If you are not an intended recipient, please
> contact the sender and destroy all copies of the original message.
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or *[log in to unmask]
> * <[log in to unmask]>
> ______________________________________________________________________
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or *[log in to unmask]
> * <[log in to unmask]>
> ______________________________________________________________________
>
>
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2