Hi Craig - if your goal is flux control then I would recommend you
eliminate the flux bottles entirely and move to a paste or "tacky" flux. A
tacky flux allows for specific application location and volume control.
With a liquid flux, you know that not all of the flux will see soldering
temperatures, especially if your operators are overzealous with its
application. With that being said, when we implemented this protocol, the
operators wanted to lynch Doug and I for about 6 months - its quite the
culture change. But in the long run, its a protocol that has worked well
and eliminated the majority of flux related defect issues/concerns.
Dave Hillman
Rockwell Collins
[log in to unmask]
From: Craig Sullivan <[log in to unmask]>
To: <[log in to unmask]>
Date: 09/20/2013 10:24 AM
Subject: [TN] Liquid Flux dispensing
Sent by: TechNet <[log in to unmask]>
This is an elementary question, but we do a fair bit of hand soldering in
some of our assemblies. We use flux bottles with needle nozzles in order
to
dispense the flux on the board. I'd like to control how much flux is
dispensed. I know training is paramount, but in my effort to give the
operators tools to do their job more effectively, can anyone point me to
items to look at? I know about flux pens and we do use them as well, but
was
just wondering what others might be using.
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480 x115
F: 607.266.0482
<mailto:[log in to unmask]> [log in to unmask]
P Please consider the environment before printing this e-mail.
_____
Confidentiality Notice:
This e-mail contains privileged and confidential information which is the
property of MPL Incorporated, intended only for the use of the intended
recipient(s). Unauthorized use or disclosure of this information is
prohibited. If you are not an intended recipient, please immediately
notify
MPL Incorporated and destroy any copies of this email. Receipt of this
e-mail shall not be deemed a waiver by MPL Incorporated of any privilege
or
the confidential nature of the information.
Export Control:
This message is intended only for the addressee and may contain
information
that is company confidential or privileged. Any technical data in this
message may be exported only in accordance with the U.S. International
Traffic in Arms Regulations (22 CFR Parts 120-130) or the Export
Administration Regulations (15 CFR Parts 730-774). Unauthorized use is
strictly prohibited and may be unlawful. If you are not the intended
recipient, or the person responsible for delivering to the intended
recipient, you should not read, copy, disclose or otherwise use this
message. If you have received this email in error, please delete it, and
advise the sender immediately.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|