Rex,
But isn't the down side of too little flux really bad? I am thinking
opens?
I think the real issue here is about cleaning after hand re-work. For that
I don't have much of an answer.
For a lab environment I played with one of those water jets used for teeth
cleaning. On the occasional rework you fill the plastic container with
distilled water, 45 seconds in the microwave, place container in holder, and
then you get a good jet of hot distilled water to clean under parts.
Yes, a total hack but it works better than ... not cleaning at all! But
this does means folk are reworking with water soluble which is a very risky
idea from the start. But if you want cosmetically appealing hand rework I
don't know of other ideas.
So "Let them have Flux" but clean well.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Hansatech
Sent: Friday, September 20, 2013 9:41 AM
To: [log in to unmask]
Subject: Re: [TN] Liquid Flux dispensing
We banned flux bottles due to the frequent over fluxing that resulted. The
level of skill required to prevent surplus flux was too great to risk it. We
now only use pens.
Regards
Rex
Sent by me on my iPhone.
On 20 Sep 2013, at 16:23, Craig Sullivan <[log in to unmask]> wrote:
> This is an elementary question, but we do a fair bit of hand soldering
> in some of our assemblies. We use flux bottles with needle nozzles in
> order to dispense the flux on the board. I'd like to control how much
> flux is dispensed. I know training is paramount, but in my effort to
> give the operators tools to do their job more effectively, can anyone
> point me to items to look at? I know about flux pens and we do use
> them as well, but was just wondering what others might be using.
>
>
>
> Craig Sullivan
>
> Manufacturing Engineer
>
> MPL Incorporated
>
> P: 607.266.0480 x115
>
> F: 607.266.0482
>
> <mailto:[log in to unmask]> [log in to unmask]
>
> P Please consider the environment before printing this e-mail.
>
>
>
> _____
>
> Confidentiality Notice:
> This e-mail contains privileged and confidential information which is
> the property of MPL Incorporated, intended only for the use of the
> intended recipient(s). Unauthorized use or disclosure of this
> information is prohibited. If you are not an intended recipient,
> please immediately notify MPL Incorporated and destroy any copies of
> this email. Receipt of this e-mail shall not be deemed a waiver by MPL
> Incorporated of any privilege or the confidential nature of the
information.
>
> Export Control:
> This message is intended only for the addressee and may contain
> information that is company confidential or privileged. Any technical
> data in this message may be exported only in accordance with the U.S.
> International Traffic in Arms Regulations (22 CFR Parts 120-130) or
> the Export Administration Regulations (15 CFR Parts 730-774).
> Unauthorized use is strictly prohibited and may be unlawful. If you
> are not the intended recipient, or the person responsible for
> delivering to the intended recipient, you should not read, copy,
> disclose or otherwise use this message. If you have received this
> email in error, please delete it, and advise the sender immediately.
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|