TECHNET Archives

September 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 13 Sep 2013 07:58:00 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (185 lines)
Picture has been sent to Steve.  I wonder if this will work.

Doug Pauls





From:   "David D. Hillman" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   09/13/2013 07:18 AM
Subject:        Re: [TN] Gull wing solder joints and minimum electrical 
clearance
Sent by:        TechNet <[log in to unmask]>



Hi Victor - I don't have an example of what happens to a QFP as Ian 
detailed but  Doug and I have the same phenomenon for a BGA.   Hey Doug - 
can ya send Steve one of the BGA pictures?


Dave Hillman
Rockwell Collins
[log in to unmask]



From:   Victor Hernandez <[log in to unmask]>
To:     <[log in to unmask]>
Date:   09/13/2013 05:50 AM
Subject:        Re: [TN] Gull wing solder joints and minimum electrical 
clearance
Sent by:        TechNet <[log in to unmask]>



Can you share this phenomenon photo?
Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fox, Ian
Sent: Friday, September 13, 2013 2:39 AM
To: [log in to unmask]
Subject: Re: [TN] Gull wing solder joints and minimum electrical clearance

Here's a phenomenon that can occur Richard. On fine pitch QFPs with a 
generous volume of solder in the joint or a bulging joint, the presence of 

a reasonable thickness of acrylic conformal coating (say 100um) between 
the feet of the device, together with regular extended periods of time 
below zero degC (say -10 degC) can result in the solder being extruded out 

of the joint thus forming a short to the adjacent lead. The modulus of the 

acrylic is greater than that of the SnPb at sub zero temps so the solder 
is under compression and flows.

Been there and got that particular T-shirt

Regards
Ian

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 11 September 2013 20:03
To: [log in to unmask]
Subject: Re: [TN] Gull wing solder joints and minimum electrical clearance

Joyce, how would it affect reliability?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Wednesday, September 11, 2013 1:18 PM
To: [log in to unmask]
Subject: Re: [TN] Gull wing solder joints and minimum electrical clearance

More likely effect your reliability than electrical clearance.

Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong
Sent: Wednesday, September 11, 2013 2:06 PM
To: [log in to unmask]
Subject: [TN] Gull wing solder joints and minimum electrical clearance

We have assemblies where gull wing solder joints have so much solder that 
along the side joint, the solder connection extends out to the adjacent 
leads similar to Figure 5-1, Image C from IPC-A-610E.  "the solder 
connection to a termination may exhibit a wetting angle exceeding 90 
degrees when it is created by the solder contour extending over the edge 
of the solderable termination area or solder resist" (We will be modifying 

our stencils to reduce the amount printed on these parts in the future).

There is no IPC-610 spec for this condition so we were thinking that if 
the spacing between the solder joints does not violate Minimum Electrical 
Clearance, they are acceptable.

Is this a correct acceptability criteria?

Thanks,
Peter

________________________________
The enclosed documents are proprietary items to Silicon Forest 
Electronics' (SFE) customers. They shall not be reproduced nor disclosed 
for any purpose except as specified in writing from an authorized agent of 

SFE. These documents may contain data restricted for export by the 
International Traffic in Arms Regulations (ITAR) section of the Arms 
Export Control Act (or the Export Administration Act). Violators are 
subject to severe criminal penalties.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 

information. Any use of this information by anyone other than the intended 

recipient is prohibited. If you have received this transmission in error, 
please immediately reply to the sender and delete this information from 
your system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be 
unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned.

______________________________________________________________________
Aero Engine Controls is part of the Rolls-Royce Group, whose legal entity 
is Rolls-Royce Engine Control Systems Limited which is registered in 
England.

Registered office at Moor Lane, PO Box 31, Derby, DE24 8BJ. Company number 

6686268, UK VAT number GB 939 396 075

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2