Hi George!
Got it up! It's here:
http://stevezeva.homestead.com/Creature_Caused_Failures.pdf
Was trying to think of something witty to say about the Gecko and Geico
car insurance but couldn't think of anything....hehehe
Steve
-----Original Message-----
From: Wenger, George M. [Contractor]
[mailto:[log in to unmask]]
Sent: Thursday, September 19, 2013 10:17 AM
To: TechNet E-Mail Forum; [log in to unmask]; Steve Gregory
Subject: RE: Bug / Insects skeletal
Victor,
In the past 13 years I had the opportunity to document three creature
caused failures of telecommunication products. I've attached
photographs of the three creatures (snake, ant, and gecko) and have
copied Steve in hopes that he will post the photos for others to see.
We believe the creatures were alive when they caused a short-circuited
and failed the electronics and died by electrocution. We know this
might be viewed as cruel and unusually punishment by some but we viewed
the creatures were trespassing. Our customers weren't upset at what
happened to the creatures but they were glad that we were able to
identify the root cause for the failures.
Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home (732) 309-8964 Mobile
E-mail: [log in to unmask]
[log in to unmask]
-----Original Message-----
From: Wenger, George M. [Contractor]
Sent: Thursday, September 19, 2013 10:21 AM
To: 'TechNet E-Mail Forum'; [log in to unmask]
Subject: RE: Bug / Insects skeletal
Yes absolutely.
Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home (732) 309-8964 Mobile
E-mail: [log in to unmask]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Thursday, September 19, 2013 9:05 AM
To: [log in to unmask]
Subject: [TN] Bug / Insects skeletal
Fellow TechNetters:
Can the remains of Insects/Bugs skeletal on the surface of a
motherboard cause a functional failure before they died?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|