Sender: |
|
X-To: |
|
Date: |
Wed, 4 Sep 2013 21:36:36 +0800 |
Reply-To: |
|
Message-ID: |
|
Subject: |
|
From: |
|
Content-Transfer-Encoding: |
quoted-printable |
In-Reply-To: |
|
Content-Type: |
text/plain; charset="utf-8" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Lyon Yuan
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of Lyon Yuan
Sent: Wednesday, September 04, 2013 9:32 PM
To: [log in to unmask]
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Hi Ben,
I send a clear picture for your reference
Lyon Yuan
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Wednesday, September 04, 2013 8:04 PM
To: [log in to unmask]
Subject: Re: [TN] EXTERNAL: [TN] BGA pad drop
Lyon,
I haven’t seen that.
Typically the pads on the BGA are solder mask defined, which makes them much more secure than the usual non-solder mask defined pads on the PWB.
Ben
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, September 04, 2013 7:04 AM
To: Gumpert, Ben
Cc: TechNet
Subject: Re:Re: [TN] EXTERNAL: [TN] BGA pad drop
hi ben,
it is pad missing from bga
在2013/09/04, "Gumpert, Ben" < <mailto:[log in to unmask]:[log in to unmask]> [log in to unmask]<mailto:[log in to unmask]>> 写道:
Lyon, By 'pad drop' do you mean lifted pads? (Pads stayed with the BGA?) Usually this means that there wasn't enough heat - that the solder was not melted in all locations. Ben -----Original Message----- From: TechNet <mailto:[mailto:[log in to unmask]]> [mailto:[log in to unmask]] On Behalf Of Lyon Yuan Sent: Wednesday, September 04, 2013 6:40 AM To: <mailto:[log in to unmask]:[log in to unmask]> [log in to unmask]<mailto:[log in to unmask]> Subject: EXTERNAL: [TN] BGA pad drop guys,we found a few BGA pad drop after removed from pcba boards.what is reason to cause the issue ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]:[log in to unmask]> [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]:[log in to unmask]> [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]> [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or <mailto:[log in to unmask]> [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|