Hi Richard
Not sure on the reliability issues relating to silicone but what you do tend to get with silicone based tapes is a de wetting effect. Is this only cosmetic in nature? I guess it's a question of the inspection criteria you are using. In the end we try and avoid it as it tends to require touch up which can lead to problems in itself.
A good example of what occurs is in one of the images in the database at http://www.nexus3c.com/conformal-coating-defects-database
It shows dewetting around masking dots on a perfectly clean pcb.
Sent from my iPad
On 6 Aug 2013, at 20:17, "Stadem, Richard D." <[log in to unmask]> wrote:
> Do you think the silicone adhesive on Kapton and Shercon tapes can create a manufacturing issue during conformal coating or for sensitive electronics?
> Doug, I would be especially interested in your respected input on this question.
>
> This message and/or attachments may include information subject to GDC4S S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed only by authorized recipients. Use, storage and transmission are governed by General Dynamics and its policies. Contractual restrictions apply to third parties. Recipients should refer to the policies or contract to determine proper handling. Unauthorized review, use, disclosure or distribution is prohibited. If you are not an intended recipient, please contact the sender and destroy all copies of the original message.
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|