Myth? Not really. Too bad google wouldn't pull out the tech report prior to 90s.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Inge Hernefjord [mailto:[log in to unmask]]
Sent: Sunday, August 11, 2013 06:48 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Silicone adhesives on tapes
Partly a myth, Bev. Like 'who is afraid of..'
Inge
On 11 August 2013 20:20, Bev Christian <[log in to unmask]> wrote:
> Rich and others,
> Some more history: Short chain silicones would also creep across a PCB and
> get into mechanical switches and in the little spark that formed just as
> the
> switch was closing the silicone molecules would decompose to form silica,
> another really good insulator that would NOT get out of the way.
>
> Bev
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
> Sent: Saturday, August 10, 2013 2:07 PM
> To: [log in to unmask]
> Subject: Re: [TN] Silicone adhesives on tapes
>
> I only have seen some "suspected" occurrence of this.
>
> Somewhat dependant on how much is deposited, was the tape baked, and if you
> have an aromatic solvent based coating. The latter can extract some
> adhesive
> from the tape perimeter.
>
> You can however use Si based tape and never have issues.
>
> I personally think that is tendency to over react to the term silicone.
> That is due to hand-soldering where we all learn that silicone hand lotions
> hamper solderability (which they can), and older Si Ccings that use some
> rather obsolete cure catalyst mechanisms.
>
> Rich Kraszewski
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: Tuesday, August 06, 2013 8:18 AM
> To: [log in to unmask]
> Subject: [TN] Silicone adhesives on tapes
>
> Do you think the silicone adhesive on Kapton and Shercon tapes can create a
> manufacturing issue during conformal coating or for sensitive electronics?
> Doug, I would be especially interested in your respected input on this
> question.
>
> This message and/or attachments may include information subject to GDC4S
> S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed
> only by authorized recipients. Use, storage and transmission are governed
> by
> General Dynamics and its policies. Contractual restrictions apply to third
> parties. Recipients should refer to the policies or contract to determine
> proper handling. Unauthorized review, use, disclosure or distribution is
> prohibited. If you are not an intended recipient, please contact the sender
> and destroy all copies of the original message.
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|