Agree. Silicone is possibly the only one that can withstand leadfree reflow temperature... but you need a good silicone adhesive. If you intended to mask, it should be consider at the design stage how to keep your sensitive stuff away, not after thoughts. (nitty gritty detail counts - pay big... but not seen by many design it and throw it over the wall to CM).
Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Tuesday, August 06, 2013 1:30 PM
To: [log in to unmask]
Subject: Re: [TN] Silicone adhesives on tapes
Acrylic tapes have their own troubles: The cohesion is not as good as silicone, so you can get globs of it coming off and contaminating your work and all of your tooling. It doesn't cause dewetting, but it can cause other problems. Post-It notes and that removable Scotch tape are the worst culprits. Most plating shops I've been in use silicone on polyester carrier. It appears that their standard cleaning techniques are adequate for removing any residue.
Only time I saw actual globs of DuPont Kapton adhesive come off was when I tried to use it to mask off some copper which had been adhesion promoted with CobraBond.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, August 06, 2013 12:00 PM
To: [log in to unmask]
Subject: Re: [TN] Silicone adhesives on tapes
Thanks to all of you who have responded. This was very helpful!
From: lduso - Diamond-MT.com [mailto:[log in to unmask]]
Sent: Tuesday, August 06, 2013 10:45 AM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: Re: [TN] Silicone adhesives on tapes
We see it often. The silicone adhesive may cause dewetting around the edges of the tape or tape dots. Sometimes this can be desirable to keep the coating off the masking making it easier to remove. Some coatings exhibit no dewetting what-so-ever. As Doug would say, it depends.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com<http://www.Diamond-mt.com>
On Tue, Aug 6, 2013 at 9:17 AM, Stadem, Richard D. <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Do you think the silicone adhesive on Kapton and Shercon tapes can create a manufacturing issue during conformal coating or for sensitive electronics?
Doug, I would be especially interested in your respected input on this question.
This message and/or attachments may include information subject to GDC4S S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed only by authorized recipients. Use, storage and transmission are governed by General Dynamics and its policies. Contractual restrictions apply to third parties. Recipients should refer to the policies or contract to determine proper handling. Unauthorized review, use, disclosure or distribution is prohibited. If you are not an intended recipient, please contact the sender and destroy all copies of the original message.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|