TECHNET Archives

August 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum ([log in to unmask])" <[log in to unmask]>
Date:
Thu, 22 Aug 2013 18:28:00 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Louis Hart <[log in to unmask]>
Message-ID:
Subject:
From:
Louis Hart <[log in to unmask]>
X-cc:
Russell Dudek <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (19 lines)
TechNetters, back with another question...

One of my colleagues, copied on this email, is looking for a new rectifier for our DC copper plating line. The ones we have now get calibrated from 0 Volts - 6 volts, 0 amperes - 1000 amperes.  Ripple voltage is specified as 5% RMS of rated output.

Would anyone suggest a source for such a rectifier? Let me know if I have left out any critical information.

Louis Hart
Compunetics
Monroeville, PA
USA
[log in to unmask]<mailto:[log in to unmask]>
412-858-1232


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2