We do the same. We use magnet wire.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Tuesday, August 06, 2013 12:56 PM
To: [log in to unmask]
Subject: Re: [TN] adhesive coated wire for rework
Bruce,
first a uniqum. I've practised. This is a VERY challenging repair method.
Not for people without patience and sharp eyes.
Second, we used a mod wire which had a insulation that was melted and left a tinned and solderable wire. Used for military equipments. Can call my friends for details if you are interested.
Inge
On 6 August 2013 18:32, Nowland, Russell Howard (Russell) < [log in to unmask]> wrote:
> Bruce,
>
>
> Here is what we use.
>
> http://www.preleg.com/
>
>
>
> RUSSELL NOWLAND
> ALCATEL-LUCENT
> REPAIR STRATEGY & SUPPLIER MANAGEMENT
> 14000 Quail Spring Parkway, Suite 100
> Oklahoma City, OK 73134
> T: +1 405 302 1660
> F: +1 405 302 1622
> M: +1 405 203 0034
> [log in to unmask]
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of <Bruce Tostevin>
> Sent: Tuesday, August 06, 2013 10:47 AM
> To: [log in to unmask]
> Subject: [TN] adhesive coated wire for rework
>
> Many years ago at another company for rework and ECOs we used adhesive
> coated wire which was bonded to the card by running a special iron
> with a notched tip along its length. It was a neat, clean, easily
> reworkable alternative to Tak Pak. Recently I ran into an application
> where this might have worked nicely, but in asking around I couldn't
> find anyone who's using this technology. I know the wire was of course
> more expensive and another comment was that it was large and maybe
> more difficult to find in smaller gauges. Is anyone using adhesive
> coated insulated wire and what are / were your experiences with it? Is it suitable for high-rel applications?
>
> Bruce Tostevin
> Benchmark Electronics
> Nashua, New Hampshire
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|