TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Tue, 30 Jul 2013 21:52:36 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (98 lines)
What size is your solder ball?
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Theodore J Tontis [mailto:[log in to unmask]]
Sent: Tuesday, July 30, 2013 03:27 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter

If I understand correctly the same ball that has 30% voiding in it is the same ball that is oversized? If this is correct, than I would think the excessive voids are contributing the increased appearance of the ball. That would mean that you have the same solder volume as the other balls due to the voids taking up the volume the solder would have taken up had the voids not been there.

Ted T

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Tuesday, July 30, 2013 2:12 PM
To: [log in to unmask]
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter

Dave,

The board only failed our X-ray inspection parameters of void size and overall diameter.  We never built up the assembly, so electrical testing wasn't performed.  I highly doubt this would ever cause a problem, but we're not allowed to ship it nor rework according to customer requirements.

There are no microvias in the pads of which I'm aware, but I'll double check to make sure.

Thanks for your input!

Leland

From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, July 30, 2013 2:25 PM
To: TechNet E-Mail Forum; Leland Woodall
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter

Hi Leland - I love the supplier's comment as the existence of the 30% void demonstrates the statement to not be true. Was the 30% void an observation or was it associated with an component failure? Do you have open microvias in the pads? Also -  the JSTD-001 committee is revising the BGA void criteria to 30% based on a series of test results submitted to the committee.

Dave



From:        Leland Woodall <[log in to unmask]<mailto:[log in to unmask]>>
To:        <[log in to unmask]<mailto:[log in to unmask]>>
Date:        07/30/2013 01:19 PM
Subject:        [TN] Singular 30% Void and Oversize Ball Diameter
Sent by:        TechNet <[log in to unmask]<mailto:[log in to unmask]>>
________________________________



Folks,

We run thousands of boards a day, and almost every one carries a BGA.  We inspect each with inline X-ray.

Last week, we had one single ball to fail for a 30% void and an oversize diameter.  We contacted the supplier, and they said their process was incapable of sending out such a defect.

We've never had a void over 5%, and even those are incredibly rare.

What within our process might have caused this, and do you agree with the statement of the supplier?  How do you recommend we analyze the failure?

Thanks in advance for your help!

Leland

________________________________

"Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments."

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________


________________________________

"Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments."

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2