TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 30 Jul 2013 13:25:14 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Hi Leland - I love the supplier's comment as the existence of the 30% void 
demonstrates the statement to not be true. Was the 30% void an observation 
or was it associated with an component failure? Do you have open microvias 
in the pads? Also -  the JSTD-001 committee is revising the BGA void 
criteria to 30% based on a series of test results submitted to the 
committee. 

Dave



From:   Leland Woodall <[log in to unmask]>
To:     <[log in to unmask]>
Date:   07/30/2013 01:19 PM
Subject:        [TN] Singular 30% Void and Oversize Ball Diameter
Sent by:        TechNet <[log in to unmask]>



Folks,

We run thousands of boards a day, and almost every one carries a BGA.  We 
inspect each with inline X-ray.

Last week, we had one single ball to fail for a 30% void and an oversize 
diameter.  We contacted the supplier, and they said their process was 
incapable of sending out such a defect.

We've never had a void over 5%, and even those are incredibly rare.

What within our process might have caused this, and do you agree with the 
statement of the supplier?  How do you recommend we analyze the failure?

Thanks in advance for your help!

Leland

________________________________

?Confidentiality Notice:
This transmission (including any attachments) may contain confidential 
information belonging to the sender and is intended only for the use of 
the party or entity to which it is addressed. If you are not the intended 
recipient, you are hereby notified that any disclosure, copying, 
distribution, retention or the taking of action in reliance on the 
contents of this transmission is strictly prohibited. If you have received 
this transmission in error, please immediately notify the sender and erase 
all information and attachments.?

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2