TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lyon Yuan <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lyon Yuan <[log in to unmask]>
Date:
Tue, 23 Jul 2013 18:47:43 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (121 lines)
Thanks, Francesco

Lyon Yuan

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of Francesco Di Maio
Sent: Monday, July 22, 2013 9:41 PM
To: [log in to unmask]
Subject: Re: [TN] Regarding on press-fit connector lifted

Hello Lyon,

You may look to the IPC A-610E at chapter 4.3.2 pag. 4-15 for references on lifted pads for press-fit.

Regards.
Francesco
Francesco Di Maio
IPC e Formazione
Via Kennedy Ingresso 2, 20871 Vimercate (MB) - Italy
Desk: +39.039.639.5921 - Mobile: +39.335.5693650 - Fax: +39.039.639.5051 E-Mail:[log in to unmask]

GEST Labs S.r.l. a Socio Unico
Societa’ soggetta a direzione e coordinamento da parte di SEM S.r.l. ai sensi dell’Art. 2497 bis c.c.
Codice Fiscale, Partita IVA e Registro delle Imprese di Milano N
07602270964 – N. R.E.A. 1970226 - Capitale sociale € 500.000 interamente versato Sede Legale: Piazza Santa Maria Beltrade,.2 - 20123 Milano - Uffici Amministrativi e Stabilimento di Vimercate Via Lecco, 61 20871 Vimercate MB  

Please visit us at: www.GESTLabs.it  and  www.SemTechnologies.it

<< Rispetta l'ambiente. Non stampare questa mail se non è necessario >>
------ CONFIDENTIALITY & PRIVACY NOTICE ------ This e-mail message and any file transmitted with it, contains confidential or proprietary information. 
If you are not the intended recipient of this e-mail, please be informed that any use of the content hereof is prohibited. 
You are requested to notify immediately the sender and delete the content you received. 



"Stadem, Richard D." <[log in to unmask]> Sent by: TechNet <[log in to unmask]>
22/07/2013 15.13
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D."    <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
Re: [TN] Regarding on press-fit connector lifted






Perhaps no response because I, for one, do not understand what you are 
asking. Is the connector not flush to the PWB? Or is there a lifted pad? 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lyon Yuan
Sent: Saturday, July 20, 2013 7:33 PM
To: [log in to unmask]
Subject: Re: [TN] Regarding on press-fit connector lifted

Any reply?

Lyon Yuan


-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] On Behalf Of 
Lyon Yuan
Sent: Saturday, July 20, 2013 7:11 PM
To: [log in to unmask]
Subject: [TN] Regarding on press-fit connector lifted
Importance: High

Hi Folks,

 

What's the standard on press-fit connector lifted?

 

Lyon Yuan

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2