Hi Victor - no, it is not self limiting and bright tin plating is a
wonderful tin whisker generator!
Dave Hillman
Rockwell Collins
[log in to unmask]
From: Victor Hernandez <[log in to unmask]>
To: <[log in to unmask]>
Date: 07/17/2013 08:51 AM
Subject: [TN] Bright tin Plating, electrolytic plating
Sent by: TechNet <[log in to unmask]>
Fellow TechNetters:
Is electrolytic bright tin plating self-limiting in thickness?
Victor,