I don't know if it is considered a best practice but I have used brass, stainless steel, and aluminum sheet stock to make various types of masks for heat protection during rework operations. Typically the low static Kapton would be used to anchor the shields down where possible.
Generally this is only done if there is a heat sensitive component near the area being reworked using smt rework equipment and not for the purpose of accidental solder splashes.
When I have to perform dynamic wave rework, we typically use the Kapton to mask off/protect the surrounding area.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Thursday, July 11, 2013 8:50 AM
To: [log in to unmask]
Subject: [TN] Best Practice Question - Rework
Folks,
I was asked this morning if anyone out there utilized any type of protective board cover while rework was being performed to their assemblies. Their notion was that using such might prevent an accidental solder splash or ball from dropping into an area and it going undiscovered.
Does such an animal exist?
I know it would be awkward and cumbersome, and would be met with a lot of resistance from people who actually perform the operation...
Thanks for your help!
Leland
________________________________
“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|