Hi Wayne - One of my mentors always stated " a single random failure does
not constitute a trend". It is sometimes hard to convince a customer of
that rationale.
Dave
From: Wayne Thayer <[log in to unmask]>
To: <[log in to unmask]>
Date: 07/31/2013 06:27 AM
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter
Sent by: TechNet <[log in to unmask]>
In a high quality operation, all failures are supposed to be rare events.
If you don't look at these very carefully and treat them as precious,
they will quickly multiply and overwhelm you.
This means investigation, but as I presume you are pointing out, it
probably doesn't warrant a herculean effort with just one example. But it
does mean pretty thorough documentation in case it happens again.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerr, Bryan (UK)
Sent: Wednesday, July 31, 2013 3:04 AM
To: [log in to unmask]
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter
Hi Leland
Seems like a random event to me if you are running thousands of boards a
day. Even a minute trace of some volatile material on the ball or PEC pad
could cause this. Perhaps not worth losing sleep over and put it in the
memory banks !
Regards
Bryan Kerr
Principal Quality Engineer
CMA Lab and Process Engineering
BAE Systems Maritime Services
Manufacturing Hillend
Hillend Industrial Estate
Hillend
Nr Dunfermline
Fife
Scotland
KY11 9HQ
01383-836097
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: 30 July 2013 19:18
To: [log in to unmask]
Subject: [TN] Singular 30% Void and Oversize Ball Diameter
----------------------! WARNING ! ---------------------- This message
originates from outside our organisation, either from an external partner
or from the internet.
Keep this in mind if you answer this message.
Follow the 'Report Suspicious Emails' link on IT matters for instructions
on reporting suspicious email messages.
--------------------------------------------------------
Folks,
We run thousands of boards a day, and almost every one carries a BGA. We
inspect each with inline X-ray.
Last week, we had one single ball to fail for a 30% void and an oversize
diameter. We contacted the supplier, and they said their process was
incapable of sending out such a defect.
We've never had a void over 5%, and even those are incredibly rare.
What within our process might have caused this, and do you agree with the
statement of the supplier? How do you recommend we analyze the failure?
Thanks in advance for your help!
Leland
________________________________
?Confidentiality Notice:
This transmission (including any attachments) may contain confidential
information belonging to the sender and is intended only for the use of
the party or entity to which it is addressed. If you are not the intended
recipient, you are hereby notified that any disclosure, copying,
distribution, retention or the taking of action in reliance on the
contents of this transmission is strictly prohibited. If you have received
this transmission in error, please immediately notify the sender and erase
all information and attachments.?
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
********************************************************************
This email and any attachments are confidential to the intended recipient
and may also be privileged. If you are not the intended recipient please
delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|