Ed,
I would be interested in seeing cross-sectional views of the solder joints
made with said connectors.
Bev
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Thursday, June 06, 2013 3:00 PM
To: [log in to unmask]
Subject: [TN] Dewetting on high current connector
Greetings fellow 'netters,
I have discovered a dewetting condition on high current blade connector(s)
which causes me to raise an eyebrow. I can't find any scholarly articles
discussing the long term effect such an irregular surface at the material
contact interface (photo located at
http://stevezeva.homestead.com/Terminal_de-wetting.JPG ) will have on
connection integrity at high current. This is an extreme environment
automotive application with MTBF expectations in excess of 10 years.
Any guidance and/or professional opinions would be greatly appreciated.
As always, thanks to Steve G. for sharing his webspace with us!
Ed Popielarski
Engineering Manager
[Description: FullLogo]
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0965
Cl: 949-581-6601
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.0
11188,0.033023&ctz=420&t=m&z=16&iwloc=A
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|