Hi, genious duo,
I had an old US Army report that emphasizes a lot about irradiation of
semiconductors. Now, you have to make a distinction between cleaning
semiconductors and expose them to natural irradiation as ready products.
UV/O2 is a outstanding method of cleaning any substrates, inclusive
semiconductor wafers of all kinds, because you get a cleanliness on
molecular level. And under controlled processes, the method does not cause
any harm to the target.
About semi packages and irradiation, I understand what Juice aim at, namely
a exposure to high energy partikels or photons or phonons at such a
intensity level that you exceed the band gap levels , equal to a memory
I/O status shift. I believe modern packages and semis are radiation
hardened for critical applications like for SPACE and others. If you, of
some reason, want to clean assembled boards by means of UV/Ozone, nothing
will happen.
You can take part of the report under 'Cleaning' and the title is
'UV-Ozone Cleaning of Semiconductor Surfaces'.
Steve, you are welcome to add your antique papers to Dropbox. As I said,
most was evaluated decades ago.
Inge
On 13 June 2013 17:28, Steven Creswick <[log in to unmask]> wrote:
> Joyce,
>
> I am going to send a couple old papers on plasma cleaning to Inge to see if
> he will incorporate them into his drop box. They are both 1989 vintage,
> essentially back in the olden days of plasma cleaning, so may be of little
> specific use, other than generics.
>
> If I get the time I will attempt to search through some of the 1990-2000
> ISHM/IMAPs symposiums for more info
>
> ?Thought you were on vacation ...?
>
> Steve Creswick
> Sr Associate - Balanced Enterprise Solutions
> http://www.linkedin.com/in/stevencreswick
> 616 834 1883
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
> Sent: Thursday, June 13, 2013 10:22 AM
> To: [log in to unmask]
> Subject: Re: [TN] Dropbox
>
> Inge, any study regarding the potential damage of memory by UV ozone?
> Especially, programmables. Thx.
> --------------------------
> Sent using BlackBerry
>
>
> ----- Original Message -----
> From: Inge Hernefjord [mailto:[log in to unmask]]
> Sent: Thursday, June 13, 2013 09:37 AM
> To: [log in to unmask] <[log in to unmask]>
> Subject: [TN] Dropbox
>
> / Cleaning
>
> added
>
> 1. Relative Etch rate in Fluorcarbon Plasmas
>
> 2.UV/Ozone Cleaning of Surfaces
>
> 3. Very Low Temperature Ashing (VLTA)
>
> Old information, still actual, but hard to find. Most about cleaning was
> done more than 20 years ago. The Cyprus guru knows. He has written a good
> book that is permanently on my desk.
>
> Inge
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute non-public
> information. Any use of this information by anyone other than the intended
> recipient is prohibited. If you have received this transmission in error,
> please immediately reply to the sender and delete this information from
> your
> system. Use, dissemination, distribution, or reproduction of this
> transmission by unintended recipients is not authorized and may be
> unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|