TECHNET Archives

June 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 24 Jun 2013 13:42:36 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Message-ID:
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Pat,
I was not being critical of your method, because I'm sure you did your homework and assessed such things as the hull effect or otherwise your repair job could leave a yacht to be desired.
I was just mentioning that many things need to be considered, prior to determining an adhesive for the job.
Dewey

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Friday, June 21, 2013 9:58 PM
To: Whittaker, Dewey (EHCOE)
Subject: RE: [TN] circuit board repair materials

Dewey,

The method I described below is how I was taught in 1976 in Uncle Sam's Yacht and Canoe Club micro circuit board repair course taught by Pace. 
I believe the adhesive of choice then was Armstrong, but Barco Bond is 
now what I have provided.   I have also used fiberglass resin and fiber 
but that is way tooooooo messy for a small repair that may not be structural.
Form, Fit, and Function.

Phil, The other adhesives group that may be worth a look at is Master Bond Adhesives, they make a lot of adhesives for the electronics industry.

pat

On Fri, Jun 21, 2013 at 9:19 AM, Whittaker, Dewey (EHCOE) wrote:

> I don't know you two, but you have my dipoles in a bind just thinking 
> about it. I have done a lot of engineering work on the development and 
> use of adhesive in the Aerospace Industry. Patents and procedures 
> aside, there is a lot of testing and environmental impacts to assess.
> Brian makes good points, as the both of us being old  war horses, it 
> is an uncomfortable expectation of familiarity with glue factories. If 
> this is just filling a void, with no functional expectations then the 
> choice is much easier. Any required functional (electrical,
> structural) characteristics demands more Dewey diligence in the choice 
> of adhesives.  Dewey -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Pat Goodyear
> Sent: Friday, June 21, 2013 8:26 AM
> To: [log in to unmask]
> Subject: Re: [TN] circuit board repair materials
>
> Phil,
>
> I use Barco Bond M-100X as the base, I also will grind up some circuit 
> board to add to the adhesive to give the fill some board body if the
> area is large.   There is usually some unused portion of the board 
> that using a rasp one can obtain enough filler material to do the job 
> to add it to adhesive.   You can also mill out the area, and using a 
> piece of scrap board mill a patch and epoxy it in place.  I have done 
> it both ways and it depends on the size of the divot.
>
> Pat Goodyear
>
>
> On Fri, Jun 21, 2013 at 6:20 AM, Nutting, Phil wrote:
>
>> Good morning all,
>>
>> This is a question regarding the repair of FR-4 after there has been 
>> a high voltage arc/burn.  In a recent failure we ground out all the 
>> burned material and "repaired" the board with 5 minute epoxy.  This 
>> is on a pancake connector for a 160kV x-ray tube.  I am of the 
>> opinion that 5 minute epoxy will soon fail as it does not have the 
>> same insulating characteristics as the base FR-4.
>>
>> I see that Circuit Technology carries all sorts of repair 
>> materials/kits.  So, if you were to salvage a burnt circuit board 
>> that had to ship right away, what materials would you use?
>>
>> Off line replies are accepted if you want to protect your sources or 
>> don't want to "advertise" on Technet.
>>
>> Thanks in advance for your wealth of information,
>>
>> Phil Nutting  |  HVP Development Engineer   |  Excelitas Technologies 
>> Corp
>>
>> Office: +1 978.224.4152
>> 35 Congress St, Salem, MA  01970 USA
>> [log in to unmask]<mailto:[log in to unmask]>
>> www.excelitas.com<http://www.excelitas.com/>
>>
>>
>> [Excelitas R_emailsig]
>>
>>
>> Please consider the environment before printing this e-mail.
>> ________________________________
>> This email message and any attachments are confidential and 
>> proprietary to Excelitas Technologies Corp. If you are not the 
>> intended recipient of this message, please inform the sender by 
>> replying to this email or sending a message to the sender and destroy 
>> the message and any attachments. Thank you.
>>
>>
>>
>> 
>> _____________________________________________________________________
>> _ This email has been scanned by the Symantec Email Security.cloud 
>> service.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>> _____________________________________________________________________
>> _
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud 
> service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2