(1) Polymer stress relaxation?
(2) You got interface problem - not bonding lock but lubrication?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Ed Popielarski [mailto:[log in to unmask]]
Sent: Wednesday, May 15, 2013 11:57 AM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] Elastic/plastic deformation of thermoplastic transistor housing
I have run across an interesting phenomenon and was hoping someone has done exhaustive research on it in Technet-ville.
I have a TO-3PF style package (plastic power transistor with plastic tab) that has a specific torque requirement and thread-locker material (microsphere type). When the subassembly is first assembled in a fixture to align the transistors to the heatsink and hold the nut in rotational place then torqued, they are verifiably tightened correctly. Once they sit for a day or so, they are no longer tight and the screw/nut spins in situ together. To my amateur eye, it seems the thermoplastic is exhibiting elastic deformation at this point. If re-torqued again, it stays put, which seems to possibly have crossed the threshold from elastic deformation ("bending" the atomic structure) to plastic deformation ("shearing" the atomic structure).
Is there any insight I can harvest before my 1:00 meeting today?
Ed Popielarski
Engineering Manager
[Description: FullLogo]
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0965
Cl: 949-581-6601
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|