TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Date:
Wed, 8 May 2013 15:49:50 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (140 lines)
You cut open the bottom part of the can so that you can crush it.

Doug Pauls



From:   Ed Popielarski <[log in to unmask]>
To:     <[log in to unmask]>
Date:   05/08/2013 02:57 PM
Subject:        Re: [TN] 2-part epoxy for pcb repair
Sent by:        TechNet <[log in to unmask]>



Pondering "reopen". How does one do that with a tin can?

Ed Popielarski
Engineering Manager


                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Wednesday, May 08, 2013 12:49 PM
To: [log in to unmask]
Subject: Re: [TN] 2-part epoxy for pcb repair

Sheeeze, guess I should have read the original date of the post!!!   OOOPs 
my bad, have been off a couple of weeks and was catching up on emails. 

Sorry to reopen this tin can of worms. 

pat

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Goodyear, Patrick
Sent: Wednesday, May 08, 2013 10:39 AM
To: [log in to unmask]
Subject: Re: [TN] 2-part epoxy for pcb repair

Wow amazing and timely, just got into a conversation with a fellow 
technician over this very subject yesterday.  He was looking at the film 
adhesives from Circuit Technology and I prefer to use a two part rapid set 
epoxy, due to the stated reasons. 

I believe the copy we have of 7711A/7721A recommends thermally bonded 
adhesives.   My issue is that when the land or pad is soldered to, the 
trace can shift or lift as the "glue" is heated.   I was originally 
trained using Loctite super glue with a liquid activator, however again 
when the area is heated the bonding agent sometimes releases.   I have had 
best results using BARCO BOND MB-165 quick set epoxy made by Astro 
Chemical, sets in 10-15 seconds, cures in a couple of minutes, I use their 
100X product for board repair, it has longer working and cure times, on 
the order of 20 minutes, usually will mix in some shredded board when I 
need a large fill or strength and to color match. 

I know it isn't totally what you are looking for but may be an alternate.  


Pat 
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, April 24, 2013 1:43 PM
To: [log in to unmask]
Subject: [TN] 2-part epoxy for pcb repair

Good afternoon,

 

I am drawing an absolute blank trying to remember the 2-part epoxy that 
I've used in the past for PCB repair (sheesh)!

 

Can anybody refresh my memory? The little epoxy packets from Circuit 
Technology Center are pretty pricey. I remember that I used something 
else, but can't remember what it was?

 

Thanks!

 

Steve Gregory

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit 
http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit 
http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2