TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M. [Contractor]" <[log in to unmask]>
Date:
Wed, 1 May 2013 08:00:49 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (206 lines)
Hi George - that specific BGA was quite large so optical inspection access 
to see the outer row was pretty minimal which is why we used Xray 
assessment. I have had the same success as Ed in finding HOP defects - 
Xray won't find them all but it can do a fair job most of the time 
especially if you have any form of CT capability or oblique angle viewing. 
We used cross sectioning to confirm what we had found using Xray 
assessment. I'll sent the photo to Steve for posting. And we are in 
agreement on the inspection methodology - we use xray assessment only when 
optical inspection isn't value added or we suspect that our BGA  process 
control protocols have been compromised.

Dave



From:   "Wenger, George M. [Contractor]" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   04/30/2013 08:20 PM
Subject:        Re: [TN] Pic of head-in-pillow for the site
Sent by:        TechNet <[log in to unmask]>



Hi Dave,

I'm really not a Doubting Thomas and I do believe you (because I know you) 
that the x-ray is of a HOP defect but I think it would be helpful to say 
how you know for sure that the x-ray shows a HOP defect.  I assume you 
know it is a HOP defect because you looked at it optically (i.e., with a 
mirror or fiber scope) and saw it was a HOP defect or you cross sectioned 
it an confirmed it was a HOP defect.  Do you have an optical image or 
photomicrograph of a cross section of the defect shown in the x-ray image?

The problem we've had with x-raying large high I/O count BGAs is that time 
consuming to scan all of the balls at a high enough magnification to find 
the balls that appear different from normal solder joints and once we 
identify the non-normal looking balls we not sure if the defect is a HOP 
or a non-soldered interconnection due to a solder paste stencil misprint 
or insufficient print.  When the defects are on outer rows we can usually 
tell by optical inspection what kind of defect it is. 

Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home (732) 309-8964 Mobile
E-mail: [log in to unmask]
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, April 30, 2013 5:10 PM
To: [log in to unmask]
Subject: Re: [TN] Pic of head-in-pillow for the site

Yes, the corner ball has the HOP.

Dave



From:   "Steve Gregory" <[log in to unmask]>
To:     <[log in to unmask]>
Cc:     <[log in to unmask]>
Date:   04/30/2013 04:08 PM
Subject:        RE: [TN] Pic of head-in-pillow for the site



Hi Dave!
 
Have your picture posted, it?s here:
 
http://stevezeva.homestead.com/HOP_iso1.jpg
 
It?s the corner ball, right?
 
Steve Gregory
 
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, April 30, 2013 12:43 PM
To: Steve Gregory
Subject: Re: [TN] Pic of head-in-pillow for the site
 
Steve - please post this HOP too - same type of thing as Ed's but another 
example for everyone benefit: 



Dave 



From:        Steve Gregory <[log in to unmask]> 
To:        <[log in to unmask]> 
Date:        04/30/2013 10:56 AM 
Subject:        Re: [TN] Pic of head-in-pillow for the site 
Sent by:        TechNet <[log in to unmask]> 




 

Hi Ed!



Nice image! Got it posted, it's here:



http://stevezeva.homestead.com/Head-in-pillow_X-Ray.JPG



What about the void off to the right? Is there any concern about that?



Steve Gregory

Process Engineer

Kimco Design and Manufacturing

652 N. Five Mile Road

Boise, ID 83713

(208) 322-0500 Ext. 3133



From: Ed Popielarski [mailto:[log in to unmask]] 
Sent: Tuesday, April 30, 2013 8:58 AM
To: Steve Gregory
Subject: Pic of head-in-pillow for the site



Hi Steve,



I have a good X-Ray picture of a head-in-pillow that Leland would find
helpful. If you don't mind posting it for him?



Ed Popielarski

Engineering Manager





                              970 NE 21st Ct.

                             Oak Harbor, Wa. 98277



                             Ph: 360-675-1322

                             Fx: 206-624-0965

                             Cl: 949-581-6601



https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
<https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&sp
n=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A> 




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2