TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Wed, 22 May 2013 08:27:58 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Bush, Brien" <[log in to unmask]>
Message-ID:
Subject:
From:
"Bush, Brien" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (61 lines)
We had an issue with foaming years ago. Using well water for makeup system, we decided to have it tested. We found we had a lot
Of microbes. Now we sanitize the system yearly to avoid this.

Brien Bush

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, May 21, 2013 12:13 PM
To: [log in to unmask]
Subject: Re: [TN] Another Closed-loop cleaner question...

Or reduce the amount of flux going into the system. Overspraying or excessive flux drag-out can lead to the foaming.
Sometimes if excessive rework is being done with a lot of tacky flux, etc, you will encounter foaming.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, May 21, 2013 10:02 AM
To: [log in to unmask]
Subject: [TN] Another Closed-loop cleaner question...

Morning all,



I may have already asked this once, and I think I know the answer, but I'll ask anyway.



It's not a good idea to use defoamers in a closed-loop cleaner, right?



If we're getting too much foam in the wash tank, we should add another carbon bed, correct?



Thanks to any who reply,



Steve Gregory




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

WARNING: Export Control
This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2