We had a foam issue once because one of the Manufacturing Engineers told the assemblers that it was ok to spray our canned de-fluxer over the open door of our batch cleaner.
Epic Fail!
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, May 21, 2013 11:02 AM
To: [log in to unmask]
Subject: [TN] Another Closed-loop cleaner question...
Morning all,
I may have already asked this once, and I think I know the answer, but I'll ask anyway.
It's not a good idea to use defoamers in a closed-loop cleaner, right?
If we're getting too much foam in the wash tank, we should add another carbon bed, correct?
Thanks to any who reply,
Steve Gregory
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|