TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Dale Ritzen <[log in to unmask]>
Date:
Thu, 16 May 2013 07:54:51 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee Hitchens <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Lee Hitchens <[log in to unmask]>
Content-Type:
text/plain; charset="ISO-8859-1"; format=flowed
In-Reply-To:
Organization:
SCH Technologies
MIME-Version:
1.0
Parts/Attachments:
text/plain (74 lines)
Hello Dale

I would support both the responses so far. We have customers which we 
must coat the edges for and its a real pain trying to do it with a 
robot. So much so we do it by hand!

But, 99% of our customers don't care. Moisture penetration is a valid 
point for sealing the edges if that is an issue for the laminate. I 
guess adhesion is a key factor and and how well the coating adheres / 
fills the voids  and holes in the laminate on the edge as well. Its 
another example of something that has been done for years in conformal 
coating but the true reasons are lost in the annuls of time with many 
engineers. Another factor I can throw in is that the majority of coating 
in automotive electronics is robot sprayed, they generally don't coat 
the edges and the automotive spec's and environment can be pretty harsh.

Finally, how do you intend to inspect? I am working on a project 
inspecting cables for deep penetration of the coating to act as a 
sealant and I can see you are going to have the same sort of problems we 
have. Using black light blue lights gives you too many reflections to 
see with the naked eye and an operator will go crazy trying to confirm 
the coating is there. We use single wavelength LEDs and a camera now 
which cuts out the white light factor but as you can guess its a real 
problem.

Best Regards

Lee Hitchens
Technical Director
SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk

TECHNICAL SUPPORT SERVICE
  
SCH Services Ltd offers a Technical Support Helpline to help address all issues relating to reliability. This includes contamination testing, cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
  
[log in to unmask]   +44 (0)1226 249019 (office hours & answerphone)   +44 (0)7862 253321 (out-of-hours emergency)

The opinions expressed in this e-mail are strictly those of the sender and not of SCH Services Limited. This communication may contain information which is confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). Unauthorised use, copying or disclosure of any of it may be unlawful. If you are not the intended recipient(s) please note that any distribution, copying or use of this communication or the information in it is strictly prohibited. If you have received this communication in error please notify us by e-mail or by telephone (+44 (0)1226 249019) and then delete the e-mail and any copies of it. Virus Warning - Although steps have been taken to ensure that all email and attachments are virus-free, we cannot guarantee nor be held liable.
  
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way Barnsley South Yorkshire S70 6BF


On 15/05/2013 20:08, Dale Ritzen wrote:
> Hello Technetters,
> Don't know if this has come up before or not (nothing in the archives), but we are researching any conformal coating requirements specifying that the edges - not just the surfaces - of the boards be covered. With the emergence of automated coating equipment, i.e. moving away from the spray or dunk coating processes, we are finding it hard to identify a coating machine that can do board edges. So...
>
> 1. Is there a valid need to coat the board edges, or is this simply a customer driven requirement? (I'm waiting for an "It depends..." on this one.)
> 2. Are there any IPC standards that address this specific question? J-STD-001E, section 10, covers coating to "all areas designated for coverage on the assembly drawing/documentation", and does not specifically mention board edges. I don't have copies of HDBK-830 or CC-830B for reference, so am relying on your inputs and experience with this question. I would be glad to do some reading up on this if anyone has any suggestions for white papers or other documents that cover this (pun intended).
>
> We'd really like to understand what the industry-wide requirements are for conformal coat in this regard. Might be a lost cause already as we have been getting the boards sprayed for years, so the customer is used to seeing every surface coated, including edges. But, the only spec they've quoted so far is the old Mil-I-46058C which was removed from service back in the 1990's. After reading through it though, I don't find anything that specifically addresses this question.
>
> Any feedback would be appreciated!
>
> Dale Ritzen, ASQ CQA
> Manager | Quality Group and ISO Management Representative
> _____________________________________________
> Austin Manufacturing Services
>
>   
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2