TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Wed, 15 May 2013 11:59:38 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Mike Bogden <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (150 lines)
A repair is due to damange. Rework is due to assembly error.

Just a thought.

Mike Bogden
Engineer



----- Original Message ----
From: "Stadem, Richard D." <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, May 15, 2013 1:43:46 PM
Subject: Re: [TN] Trend Analysis of Repair Usage

Yes, but not defects that require repair usage (lifted pads, damaged traces, 
etc.)

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Wednesday, May 15, 2013 1:08 PM
To: [log in to unmask]
Subject: Re: [TN] Trend Analysis of Repair Usage

Are not some "defects" considered "not rejectable", i.e., "process indicator"?

Ed Popielarski
Engineering Manager


                              970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0965
                              Cl: 949-581-6601

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Wednesday, May 15, 2013 10:55 AM
To: [log in to unmask]
Subject: Re: [TN] Trend Analysis of Repair Usage

Dean,

But isn't a defect a defect, regardless of the fix?

You may not track / trend repairs separately from rework, but they should be 
included in the overall defect trends. In some cases, the defect itself is 
enough to identify the instance as a repair, such as lifted/missing pads on a 
PCB. 


Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, May 15, 2013 10:39 AM
To: [log in to unmask]
Subject: EXTERNAL: Re: [TN] Trend Analysis of Repair Usage

Yes, for rework in 12.1, but for repair trending, nothing in 12.2.
Still looking for trend analysis.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Wednesday, May 15, 2013 9:28 AM
To: [log in to unmask]
Subject: Re: [TN] Trend Analysis of Repair Usage

J-STD-001 touches on this, 12.1. It does not tell you what to document. In a 
nutshell, it says you must document, and the user must agree with the repair 
approach. 


Guy

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, May 15, 2013 9:53 AM
To: [log in to unmask]
Subject: [TN] Trend Analysis of Repair Usage

I am trying to find out if there is an industry requirement or recommendation 
that usage of Repair Procedures be tracked and monitored? I could not find any 
information on this in IPC-7711/7721. In previous lives the number of repair 
usages was tracked, and pareto was published quarterly (number of repairs used 
versus number of total CCAs built, number of repairs used by a given CCA part 
number, number of repairs associated with a given component part number, etc.) .
Because repairs are infrequent, it is not easy to detect any trend in their 
usage, but over time the trend analysis can provide good data to detect root 
causes.
I just want to know if there is any industry standard that covers this.
I am talking about repairs, not rework. If you don't know the difference please 
do not respond.
Thanks
dean

This message and/or attachments may include information subject to GDC4S S.P. 
1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed only by 
authorized recipients. Use, storage and transmission are governed by General 
Dynamics and its policies. Contractual restrictions apply to third parties. 
Recipients should refer to the policies or contract to determine proper 
handling. Unauthorized review, use, disclosure or distribution is prohibited. If 
you are not an intended recipient, please contact the sender and destroy all 
copies of the original message.




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2