TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 1 May 2013 09:51:01 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (82 lines)
 

Hi Ed!

 

Got your pictures up! They are here:

 

http://stevezeva.homestead.com/CT_of_HIP.jpg

 

http://stevezeva.homestead.com/Photo_of_HIP.jpg

 

 

Steve Gregory

 

From: Ed Popielarski [mailto:[log in to unmask]] 
Sent: Wednesday, May 1, 2013 8:49 AM
To: Steve Gregory
Subject: 2 more for the website, please

 

Steve,

 

Attached are photomicrograph and a CT of the H-I-P defect.

 

Please post on the site if you have time.

 

Thanks in advace!

 

Ed Popielarski

Engineering Manager

 

 

                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277

 

                              Ph: 360-675-1322

                              Fx: 206-624-0965

                              Cl: 949-581-6601

 

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
<https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&sp
n=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A> 

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2