Greg,
I use this one, and I am very content. I use a temperature measuring
instrument with a thermocouple for adjusting the tip temperature.
http://www.hotery.com.tw/product_view.php?id=107&mode=412&PHPSESSID=32c6b26e2d264c62d336f40d337de1b5
Inge
On 4 April 2013 16:38, Gregg Owens <[log in to unmask]> wrote:
> Since we hand solder outside of the normal manufacturing floor, our
> technicians are requesting to use a butane soldering iron. I have no
> previous experience with this type of soldering iron. With a temperature
> setting of 1076°F it seems rather high and potentially damaging to
> resulting solder connection, insulation, people, etc.
>
>
> http://www.apexhandtools.com/brands/CF_Files/model_detail.cfm?upc=037103060976
>
> Any thoughts from experience would be most appreciated.
>
> Gregg
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________