An excellent low-outgassing two-part epoxy is Armstrong C7 resin with hardener "W".
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, April 24, 2013 3:43 PM
To: [log in to unmask]
Subject: [TN] 2-part epoxy for pcb repair
Good afternoon,
I am drawing an absolute blank trying to remember the 2-part epoxy that I've used in the past for PCB repair (sheesh)!
Can anybody refresh my memory? The little epoxy packets from Circuit Technology Center are pretty pricey. I remember that I used something else, but can't remember what it was?
Thanks!
Steve Gregory
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|