Hi team - I agree with Phil - where is the pad? It appears to be missing.
Any additional photos?
Dave
From: Phil Bavaro <[log in to unmask]>
To: <[log in to unmask]>
Date: 04/23/2013 12:44 PM
Subject: Re: [TN] QFN Pad Corrosion?
Sent by: TechNet <[log in to unmask]>
Steve,
I don't see a pad at all in the picture....much less a corroded pad.
I find it highly unlikely that only one pad had any kind of plating
problem on the part.
If the picture is actually showing a pad without any solder wetting to it,
even after removal, that raises my eyebrows more.
I would want to see the part.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, April 23, 2013 10:12 AM
To: [log in to unmask]
Subject: [TN] QFN Pad Corrosion?
Hi All,
I have another question about the QFN16 that I was talking about last
week. I was sent a photo of the bottom of one of the devices after it had
been removed from a failed board. It is here:
http://stevezeva.homestead.com/QFN16_Corrosion.jpg
It's pointing out a pad that seemed to have a lot of corrosion on it and I
was told that solder would not wet to it. I was asked what might cause
this?
My first thoughts are that the appearance might have been caused by the
rework when it was removed, and that a un-solderable intermetallic has
formed on pad but I can't say that for sure. The part is finished with
matte tin when it is supplied. When a part is tin finished, they have a
barrier nickel plate beneath the tin right?
I don't have the part in front of me, I only got sent the photo. I was
asked what my thoughts were, so I thought I'd ask my TechNet friends
too... :o)
Thanks,
Steve Gregory
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
________________________________
This message and any attachments are solely for the use of the addressee
and may contain L-3 proprietary information that may also be defined as
USG export controlled technical data. If you are not the intended
recipient, any disclosure, use or distribution of its content is
prohibited. Please notify the sender by reply e-mail and immediately
delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|