TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Ed Popielarski <[log in to unmask]>
Date:
Tue, 30 Apr 2013 09:55:22 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (83 lines)
 

Hi Ed!

 

Nice image! Got it posted, it's here:

 

http://stevezeva.homestead.com/Head-in-pillow_X-Ray.JPG

 

What about the void off to the right? Is there any concern about that?

 

Steve Gregory

Process Engineer

Kimco Design and Manufacturing

652 N. Five Mile Road

Boise, ID 83713

(208) 322-0500 Ext. 3133

 

From: Ed Popielarski [mailto:[log in to unmask]] 
Sent: Tuesday, April 30, 2013 8:58 AM
To: Steve Gregory
Subject: Pic of head-in-pillow for the site

 

Hi Steve,

 

I have a good X-Ray picture of a head-in-pillow that Leland would find
helpful. If you don't mind posting it for him?

 

Ed Popielarski

Engineering Manager

 

 

                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277

 

                              Ph: 360-675-1322

                              Fx: 206-624-0965

                              Cl: 949-581-6601

 

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn
=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
<https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&sp
n=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A> 

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2