I think I would let this go as it is. Yeah, a little more solder than you
would like to see, but it doesn't touch the component body, and I think you
would be risking more problems trying to remove this solder rather than just
leaving as it is...
Steve
P.S. I can's subscribe to TechNet from my new work email. Listserv doesn't
even acknowledge an email sent to it. Think it may have to be something that
I have to talk with the IT guy about. But I still get TechNet at my own
personal email account...
-----Original Message-----
From: [log in to unmask]
Sent: Monday, April 08, 2013 12:41 PM
To: [log in to unmask]
Cc: [log in to unmask]
Subject: FW: Photo Gallery, Steve Zeva
Steve,
Can you please post this photo for me.
Thanks,
Victor,
-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Sunday, October 07, 2012 6:09 AM
To: Hernandez, Victor G
Cc: Steve Gregory
Subject: RE: Photo Gallery
Hi Victor,
Steve has moved to a company in Florida. This is the url:
http://stevezeva.homestead.com/
I copied Steve, so now you have his new address.
Guy
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, October 05, 2012 12:14 PM
To: [log in to unmask]
Cc: [log in to unmask]
Subject: Photo Gallery
Importance: High
What is the URL address to your photo viewing site?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|