TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Gregg Owens <[log in to unmask]>
Date:
Thu, 4 Apr 2013 21:03:04 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Message-ID:
Subject:
From:
Inge Hernefjord <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (35 lines)
Greg,
 I use this one, and I am very content. I use a temperature  measuring
instrument with a thermocouple for adjusting the tip temperature.

http://www.hotery.com.tw/product_view.php?id=107&mode=412&PHPSESSID=32c6b26e2d264c62d336f40d337de1b5

Inge


On 4 April 2013 16:38, Gregg Owens <[log in to unmask]> wrote:

> Since we hand solder outside of the normal manufacturing floor, our
> technicians are requesting to use a butane soldering iron. I have no
> previous experience with this type of soldering iron. With a temperature
> setting of 1076°F it seems rather high and potentially damaging to
> resulting solder connection, insulation, people, etc.
>
>
> http://www.apexhandtools.com/brands/CF_Files/model_detail.cfm?upc=037103060976
>
> Any thoughts from experience would be most appreciated.
>
> Gregg
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2