Gregg,
Bought one of these for interns that were looking for tin whiskers on scrap cell phone boards. We tried to use this to de-solder the RF shields on those boards, as we thought that would be better than just pulling the shields off with a pliers. Of course, with either method, we didn't care about later board operation, as these were already scrap cell phones. I think we finally settled on a standard electric soldering iron with a large, flat surface to spread heat through the shield metal and pop the shield off.
I would say this butane iron was made for non-electronic soldering like small copper pipes or maybe assembling stained glass objects.
Denny Fritz
-----Original Message-----
From: Gregg Owens <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Thu, Apr 4, 2013 10:42 am
Subject: [TN] Butane Soldering Irons
Since we hand solder outside of the normal manufacturing floor, our technicians
re requesting to use a butane soldering iron. I have no previous experience
ith this type of soldering iron. With a temperature setting of 1076°F it seems
ather high and potentially damaging to resulting solder connection, insulation,
eople, etc.
http://www.apexhandtools.com/brands/CF_Files/model_detail.cfm?upc=037103060976
Any thoughts from experience would be most appreciated.
Gregg
______________________________________________________________________
his email has been scanned by the Symantec Email Security.cloud service.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|