TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Glidden, Kevin" <[log in to unmask]>
Date:
Tue, 9 Apr 2013 21:11:59 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Reuven Rokah <[log in to unmask]>
Subject:
From:
Reuven Rokah <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
Baking in Vacuum oven = less pads oxidation and faster drying


On Tue, Apr 9, 2013 at 9:00 PM, Glidden, Kevin
<[log in to unmask]>wrote:

> Someone in Technet not long ago posted up an excellent little write up
> from  Gordon Davy about water vapor and drying.  I've attached it to Phil
> and Bob.
>
> It contends vacuum ovens do nothing to increase drying rate.
>
> Drying is a function of temperature and delta between concentration of
> water in the middle versus at the surface.
>
> I presume, like any drying, the greater the surface area exposed the
> faster the drying.  I would place the PCBs (as much as possible) directly
> on racks or in card holders (on edge).
>
> -----Original Message-----
> From: Nutting, Phil [mailto:[log in to unmask]]
> Sent: Tuesday, April 09, 2013 1:01 PM
> To: [log in to unmask]
> Subject: Re: [TN] Pakeout and PCB Separators
>
> Robert,
>
> How about placing them in a vacuum chamber.  That would release all the
> moisture and definitely if you could add a little heat.  I would envision
> separating the boards with a mesh and spacer to allow the moisture to fully
> escape.  Placing a paper towel between layers might not let all the
> moisture escape.
>
> But then this is just my opinion.
>
> Phil Nutting
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
> Sent: Tuesday, April 09, 2013 12:54 PM
> To: [log in to unmask]
> Subject: [TN] Pakeout and PCB Separators
>
> Hi,
>
>
>
> Does anyone know if separators of some type between PCBs can reduce bake
> out time?
>
>
>
> If I have a stack of PCBs, and I place something like paper towels between
> PCBs, can the bake out time be reduced? I would imagine the diffusion rates
> of moisture in the paper towel material would be much higher than in solid
> PCB laminate. But, that is just a guess. Could be perfect hog wash.
>
>
>
> My problem is not with PCBs but with 30 mil sheets of plastic that feed a
> thermoforming process.  I am using PETG but I still see small bubbles in
> the material after forming. I tried a short bake out, and it helps, but I
> cannot heat very high as the 30 mil plastic sheets will easily deform. I
> need to lay them flat, heat gently, and still try to removed moisture. I
> was wondering what the best way to separate sheets and allow drying might
> be.
>
>
>
> Any Ideas?
>
>
>
> Thanks,
>
> Bob K.
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>



-- 

Best Regards,

*Reuven Rokah*

Mobile: 972-52-6012018
Tel:        972-3-9360688
Fax:          076-5100674
 <http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com

**
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2