Inge,
I LIKE the IMHO reference. May I use it elsewhere?
1. I don't disagree on microscopic bubbles but zillions is a little hard
to quantify. Bubbles are process indicators up to 0.375 zillion, but at
0.376 zillion, it is a defect. If I have very small bubbles out in the
middle of nowhere on my assembly, on top of a solder masked surface, not
exposing any leads or conductors, that bubble is never going to cause a
problem in service, as least in the aerospace environments I work with.
But if I have the zillions of small bubbles, it indicates an underlying
problem, perhaps too much moisture or volatiles in my solder mask that
could affect coating adhesion in service. How to draw the line?
2. When you talk about bubbles higher than 50% of the thickness, would
that be on the order of a 2 mil bubble in a 4 mil thick coating? If so,
how would you measure that, top to bottom or side to side?
3. I agree that when you start getting clusters of bubbles you have a
process problem, but how do you quantify a "cluster" of bubbles? Is 2 a
cluster (leave it alone Dewey)?
4. On the extension, do you mean above the surface of the surrounding
coating, i.e. a 30 mil tall bubble over a 3 mil coating?
Doug Pauls
From: Inge Hernefjord <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>,
[log in to unmask]
Date: 03/21/2013 07:05 PM
Subject: Re: [TN] Conformal Coat and Bubbles
IMHO (In My Hallucinate Opinion) :
- zillions of microscopical bubbles does not matter
- bubbles higher than 50% of the coating thickness do not matter if only
few
-bubbles higher than 50% and building clusters matters
-all bubbles with an extension 10 times the coating thickness matters
-if the above is repeated on many boards, the MRB should suspect a process
failure
-for all coatings
Inge
On 21 March 2013 16:18, Douglas Pauls <[log in to unmask]> wrote:
OK, Minions, your next question in the quest to improve J-STD-001 and
A-610 relates to bubbles in the conformal coating.
I think we can all agree that the ideal conformal coating layer contains
no bubbles or voids and is "purdy". BUT:
1. Are there bubbles in coatings in areas where they will not impact
reliability and their presence should be viewed as a "Process Indicator"?
If so, where and what limits would you use?
2. What would you classify as a bubble requiring disposition, i.e.
Becomes an actionable defect? If so, where and why?
3. Would any of your answers change depending on what KIND of coating it
is, i.e. Acrylic vs. silicone vs. Parylene?
Well, OK, that is three questions. I'm on a roll.
Doug Pauls
Chairman, IPC Cleaning and Coating Committees
Galactic Emporer
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|