To see Sn grain boundaries , don't etch. Use cross-polarizers.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, March 21, 2013 10:53 AM
To: [log in to unmask]
Subject: [TN] SAC 305 etch
What would a good etch be for etching SAC305 solder joints to enhance
viewing grain boundaries?
Thanks,
John
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|