I can not think of any unless dipping doesn't remove enough Au and Au is a possibility.
Regards,

Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (647) 495-8727
Cell: (416) 899-1882
www.sentec.ca

-----Original Message-----
From: Gregg Owens <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Tue, 12 Mar 2013 22:43:00 
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
        Gregg Owens
	<[log in to unmask]>
Subject: [TN] Mixing Solders

I have an industry friend who asked me the following question and I did not have a good enough reply. So I thought I would put it out there on TechNet.

What are the possible problems with tin dipping a gold plated contact with 63/37 then soldering it in a (PCB) board using 60/40 solder ?



2.    What arguments could I use to move away from using the 60/40 and use just the 63/37 for the product (i.e. Do you believe one has any benefit over the other)?



3.    Are you aware of any problems mixing the solder types ? (63 / 37 and 60 / 40)

Your thoughts and comments are appreciated.

Gregg Owens

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2