I should have mentioned the parts are mounted and polished , I just need a chemical etch to highlight the grain boundaries similar to what is used for SnPb solder joints. Exotic techniques are not available but am looking fore something that I can put in a wet lab.
John
Sent from my iPad
On Mar 21, 2013, at 4:37 PM, Inge Hernefjord <[log in to unmask]> wrote:
> John, I used to mold the specimen in well cured two-component Araldite, do
> the polishing with oil and diamond plastic discs to avoid contamination of
> the solder joint with polish particles. Use specimen rotating holder.Then
> wipe the stub with finest tissue to remove oil. Avoid solvents. Then
> perform a couple of minutes Argon sputtering, which will enhance the
> difference in hardness, Finally do microscopy with polarized light and a
> variable Nomarski lens, see page 119 here:
> http://bama.ua.edu/~mweaver/courses/MTE481/5_MTE481-MICROSCOPE&MODES.pdf
>
> There are many other methods of course, e.g. EDX element mapping mode,
> which I have practiced many a times.
>
> Inge
>
>
>
>
> On 21 March 2013 15:53, <[log in to unmask]> wrote:
>
>> What would a good etch be for etching SAC305 solder joints to enhance
>> viewing grain boundaries?
>>
>> Thanks,
>> John
>>
>> ______________________________**______________________________**__________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> **______________________________**__________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|